Shane, thanks for pointing that out (welder). I read QW-201 and just mentally went straight to procedures.
![red :red:](/f2/epx.png)
Incidentally, CommonArc is brilliant, wish it would catch on quicker!
Further re procedures, in instances where there may be a very large job, there's nothing in ASME IX that would prohibit numerous contractors / subcontractors to qualify its PQRs / WPSs jointly; i.e., each contractor would have its own welder(s) take part in one or several test coupons.... and each contractors representative present recording the variables on its own forms...