n5uzt,
I have used those spreadsheets on Gerald's site and have found them very helpful. I have some charts in a old book Lincoln published, "Procedure handbook of Arc Welding Design & Practice" 11th edition, copyright 1956. If I can remember where they are in that book, I'll be happy to fax you a copy of the pages that chart is on, provided I can locate them again. Email me your fax number if you are interested. I think there is also a chart that helps determine the #'s of filler/ft. that have already been deposited in a as welded condition. basically helps figure the area of the cross section based upon whether the fillet weld is convex or concave.
Gerald,
Haven't seen much of you. I guess that means you have been very busy.
Good to see you,
John Wright