The voltage will have the most affect on height and width of the weld deposit. Your penetration will be determined by the amperage. This amperage will be determined by the wire feed speed. The same amperage from a smaller diameter electrode will produce increased penetration. This can quickly be demonstrated by welding and cutting, polishing and etching two welds.