Was wondering if anyone could help me out. I was wondering the difference between NR-211-MP E71T-11 and NR-305 E70T-6 are, or at least where to find the information. and thoughts are much appreciated.
Your E70 is in the "Flat & Horizontal" section and your E71 is in the "All Position" so there is your first answer as to differences. Hope that helps, Cheers, Shane