hi ! all! i have a tweco style whip 10'-15' long and i know the company orders wrong tips and nozzles so my tip is flush with nozzle(new) i cut my liners long,like 15 -18 laps past the diffuser( 7/8-11/16) long!i am using bohler .035 &.045 solid. so i have this arcing on the tip and false start, and intermitten sputter during weld! i have told my super to hack the dang thing up with an axe! making it hard to make my bones!any help would be a +! miller cv 302 and miller feeder. good drive rolls! no volt or amp changes ! and wire setting are good to run have not a problem before!my guess is the support spring in back of gun kinked or a limp whip in which a double length of double layer shrink wrap can solve! i get the arc at tip when gun is lean to right and canted 15 deg. take the bend out with free hand no problem!
i know is limp whip but i gotta get a 360 degree op from this pig!