Code D1.5 section 5 Qualification; in Figure 5.1 "WPS Qualification or Pretest-Test Plate A (see 5.7.1)" Shows the distribution of almost all specimens needed, again almost all of them are explained and dimensioned in others figures and in case of CVN Block showing in the same figure 5.1 the minimum length of the block before obtain the CVN specimens.
My question is about the size of the macroetch specimen, wich does not show dimensions, how much is the minimum correct size of this specimen to comply with code requeriments?
Thanks.