To any of you CWI's out there- do any of you who have had a new stamp issued in the last couple of years have any problems with the way the mark is left on the paper after you use the stamp? Mine seems to not only leave the impression of the letters, but also the rectangular backing that the letters are on. It almost seems to me that the letters are not quite tall enough. Anyone have this issue? I was wondering if AWS would send me a new stamp if I requested one. Thanks
I have the new self inking stamp and it doesnt leave any border, just my name and such. It sounds like to have the old style, the newer ones are not raised, it's flat.
No it's not the old style. I got it after my 9yr in 2011. On the side of the stamp it says " Slim Stamp 1854". It just seems to me that the lettering is not raised enough to leave only that when I use it.