I don't have my D17.2 in front of me, but I know it spells out the requirements for machine and procedure quals almost clearly.
It even has pictures of test plate configurations.
The procedure qual is about ensuring your selected welding parameters are suitable for the application.
The machine qual is about ensuring your equipment is capable of replicating the same weld strength and penetration at the same parameters, weld after weld, with emphasis on RW equipment.
Have you looked at the Code?
Tim
Hello
Like the previous reply everything you need is in D17.2 for resistance welding,and also refer to your customer spec, requirements. When you qualify the machine make sure you use the material that is most difficult to weld, and the thinnest to thickest range that will more than cover the material thickness part type you have.