Like the oil spill, good PR for the oil companies. I wonder if the home owner was hunting squirrel in his back yard and up comes the bubblin' crude?
I guess I could continue with something else, but, I'll refrain....LOL!!
After reading the reports and seeing where the leak occurred, will bet a 6 pack of Diet Coke the pipeline was un-reported damage by third party during construction of this development. That is the number one cause of pipeline leaks. Corrosion is second.