Ok, here is all the information on the stainless steel Rig Job in Las Vegas, Nv. >>Weld test is on 8-13- 2013 in Phoenix, Az. and job starts on 8-15-2013 in Las Vegas, Nv.
Need 4 Rig Weldors >> 2-3 wks, 2”, 3”, 4”, 6”, 8”, 10” and 14” schd 10 S/S >> 5-10’s @ $57 on the arm $14 on rig and $100 per diem , >>Bring your helper, $41 and $100 per diem >>10 hrs travel for weldors only >> Tig wire and Argon furnished by client.
>>> Weld test- 6 -G position, 2 ½” 316L .203 WT. >> Heli-arc (Tig ) stainless all the way out
Hotels are cheap !! Sam’s town @ $28 a night !!!
Contact Skip @ 602-359-2955 between the hours of 7am and 7pm Arizona time !!