- - By magesh (*) Date 08-23-2013 15:06
HI

We performed UT Thickness check on slot welds. Now my Question is what is the tolerance for thickness material as per AWS D1.1 (The tolerance After repair the material)

Thanks
Parent - - By 803056 (*****) Date 08-23-2013 15:58
Clause 5 contains the information you are looking for.

Al
Parent - - By magesh (*) Date 08-24-2013 06:19
Sorry Please give me specific paragraph or section in clause 5.

very sorry about this i could not find the tolerances on clause 5

Thanks

Reagrds
Parent - By 803056 (*****) Date 08-24-2013 13:36
You could use 5.24.3.1. It relates to groove welds finish flush, but that is the best I can come up with. This consistent with the allowable undercut for a connection subject to static loads.

The alternative is to address the question to the Engineer. Where the code is not explicit, the Engineer, who represents the Owner,  is the individual with the authority to make a determination.