Code: D1.3 & D17.2
The weld call out in question is a fillet weld that is .400" The print references D1.3 as well as D17.2 (which is on order).
The engineer has asked me a question that I can't seem to find the answer to so I'm
1.) What is the maximum and minimum allowable leg sizes? I deal with JD code on a daily basis and it states that the leg length can be 1mm under and 3mm, with no more than 3mm between the two
legs.
2.) Is there a tolerence on the length of a weld as well per the above mentioned codes?
Thanks,