there isnt inlet/outlet ,for example ,two plants are welded on the tube or pipe to be enclose vessel ,when weld the first plant ,it isnt usually produce gas hole,because the heat gas will diffusion from the edge of pipe ,but when welding the second plant ,the heat gas cant diffusion timely,so produce the gas hole on second bead.