/ 1104 welding test pipe coupons
By
Jerry Kavalir
Date
01-30-2014 04:35
How long should the individual pieces of pipe be for the 12" open butt and 12" on 12" branch welding test be?
By
dbigkahunna
Date
01-30-2014 14:10
10-12 inches
By
Jerry Kavalir
Date
01-31-2014 02:14
Thanks dbigkahunna. I didn't know if there was a standard for the length or not.
By
jarsanb
Date
01-30-2014 18:17
And....for the piece the branch connects to (run), no less than 24". you will need enough on the test straps to grip to for your nick breaks. This will give you approximately 5.5" on each end after the branch is centered.
By
Jerry Kavalir
Date
01-31-2014 02:17
Thanks jarsanb. I appreciate the info.
By
Jerry Kavalir
Date
02-19-2014 02:23
What can anyone tell me about acceptance or rejection of a concave cover pass by 1104 standards
By
dbigkahunna
Date
02-19-2014 04:32
Bottom of the concave has to be higher than the pipe.
By
Mwccwi
Date
02-19-2014 09:57
I like your response Kahunna,
I'll have to remember it.
Topic
Welding Industry
/
Inspection & Qualification
/ 1104 welding test pipe coupons
Forum
AWS.org
- Forum News & Help
American Welding Society Services
- Certifications
- Conferences & Shows
- Technical Standards & Publications
- AWS Learning & Education
Welding Industry
- General Welding Discussion
- Technical Discussions
- Inspection & Qualification
- Processes
- Welding Fundamentals
- ASME Codes
- Welding Safety
- Metallurgy
- Welding Documents & Downloads
Welders and Inspectors
- Education & Training
- Welding Equipment Classifieds
Sections
- Section 7: San Francisco
- Section 32: Rochester
- Section 39: Colorado
- Section 41: Puget Sound Olympic
- Section 55: Arizona
- Section 81: Nebraska
- Section 110: North Florida
- Section 112: Florida West Coast
- Section 135: Nevada
- Section 156: Inland Empire
Chit-Chat & Non-Welding Discussion
- Off-Topic Bar and Grill
Powered by
mwForum
2.29.2 © 1999-2013 Markus Wichitill