Hi BM146,
A scratch start may be used in lieu of a high frequency start, and although the tungsten is briefly scratched against the work piece, there is the possibility of tungsten contamination. The arc should not be struck on a carbon block because of the likelihood of carbon contamination. Some codes do not allow scratch starts.