I have a drawing from a customer that states" weld procedures AND welders shall be qualified for CVN requirements of AWS D1.1" Is there a welder qualification that is derived from Charpy V-notch testing? The material is ASTM A572 Gr 50. Filler metal is E70C-6M using GMAW process.
I have an existing weld procedure that I can get qualified for CVN but do not know of any welder qualification requirements. Next question is that the weld procedure that I have was pre-qualified GMAW so I had no mechanical testing done at all, just the welders qualification tests were performed using it. So does having to perform CVN testing mean that I would have to get the rest of the procedure qualification testing done too? I know this is basic for some of you but I hope to learn something here.
Thanks!