Dude, someone is in serious violation of the "maximum 3 rod bead width restriction clause".
Would not hold water, aye? Did anyone test to see if it would hold sand First???
![confused :confused:](/f2/epx.png)
![razz :razz:](/f2/epx.png)
![lol :lol:](/f2/epx.png)
Tests.
1) Visual test
a) Is it ugly?
b) If so, have you ever tried to pass one off that looked as bad or worse?
2) Light test...
a) can you see your flashlight thru the weld?
b) If so, can you see your flashlight thru the weld, with it turned off?
c) Can you read the newspaper headline thru it?
If answer is no to all the above... Now you may proceed to the sand test, then followed by hydro.
Enjoy Dubai. BTW if you buy tickets online they are $25 instead of the $100 at the door price to go up in the Burg Khalif (formerly world's tallest building).
The observation deck is on the 125th floor. Crazy part is you still have the equivalent of the Sears Tower above you!!!