6 x 1/4"" 420 flat bar to 12" sch 80 309 ss
a fillet weld on to the pipe
butter the 420 end with 309 filler and then weld together with 309?
no code, but use asme, for baseline
![eek :eek:](/f2/epx.png)
![evil :evil:](/f2/epx.png)
![cool :cool:](/f2/epx.png)
on the right track?
thank you for your time and consideration
sincerely,
Kent
edit: gmaw for the buttering and smaw for the fillet
'