Hello, I have a question about weld profiles, namely T joint grove weld transitions to the plane of the base metal. 5.24.3 says "Welds shall have a gradual transition to the plane of the base-metal surfaces". Most CWI's interpret that to mean not greater than a 90 Deg angle and go to figure 5.4, So is a 90Deg transition with no reinforcement required fulfill 5.24.3