Hey guys,
We received an order to weld some 304 SST plate and tubing which we plan on using GTAW. The drawing note states to weld IAW D10.4-1986
We have never worked to 10.4 before, so I have a few questions regarding welder/procedure qualification.
I see there is quite a bit of variables to consider, but as I'm reading 10.4 (1986) the only thing I see regarding welding procedures is in Appendix A2.9 Welding Procedure Consideration which lists what appear to be variables to "consider", and also A2.16 Welder Training, which mentions certification by conventional ASME bend tests or radiography.
So if we created a WPS qualified to ASME IX, taking into consideration the variables listed in D10.4 and also essential variables listed in ASME IX, would this be acceptable per D10.4?
What other considerations should I be aware of? I don't want to "over complicate" this, but I do want to make sure we have the bases covered.