- - By Vivekbatish Date 02-01-2015 07:30
Hi Everyone,

i am trying to find out SMAW consumable for P92 material. but in AWS there is no particular consumable specification for P92 material.
Can i use E9015-B9 for P92??

Kindly suggest

Thanks in Advance..
Parent - - By js55 (*****) Date 02-02-2015 21:49
Vivek,
There are few manufacturers for material for Grade 92. I would contact Euroweld.
Parent - By fschweighardt (***) Date 02-03-2015 17:33
Most everything for the best P92 welding is going to be proprietary.  Closest AWS classification is E-90XX-B9, but that is really for P91.  Most P92 formulations will be a modification of the P91 fillers