/ 8010 stick rods
By
chingao81375
Date
08-30-2004 02:45
I have recently come across some 8010 70+ welding rods and since im just a welding novice, what would those rods be best used for. I would like to utilize them in what they were designed for. And by the way the sizes are 5/32 and 3/16.
By
ajoy
Date
08-30-2004 12:10
These electrodes are used for welding fill and cap passes of X56 to x70 gr. pipelines.
Topic
Welding Industry
/
General Welding Discussion
/ 8010 stick rods
Forum
AWS.org
- Forum News & Help
American Welding Society Services
- Certifications
- Conferences & Shows
- Technical Standards & Publications
- AWS Learning & Education
Welding Industry
- General Welding Discussion
- Technical Discussions
- Inspection & Qualification
- Processes
- Welding Fundamentals
- ASME Codes
- Welding Safety
- Metallurgy
- Welding Documents & Downloads
Welders and Inspectors
- Education & Training
- Welding Equipment Classifieds
Sections
- Section 7: San Francisco
- Section 32: Rochester
- Section 39: Colorado
- Section 41: Puget Sound Olympic
- Section 55: Arizona
- Section 81: Nebraska
- Section 110: North Florida
- Section 112: Florida West Coast
- Section 135: Nevada
- Section 156: Inland Empire
Chit-Chat & Non-Welding Discussion
- Off-Topic Bar and Grill
Powered by
mwForum
2.29.2 © 1999-2013 Markus Wichitill