- - By Harman (*) Date 02-09-2015 20:35
Guys,

Do you have recommendations for software which can help in developing weld sequence and predicting weld distortion.

Thanks
Parent - - By pipewelder_1999 (****) Date 02-11-2015 03:53
There are formulas in AWS Welding Handbook, Volume 1 that calculate "theoretical" angular distortion, transverse shrinkage and other things. I wrote some GWBAsic code many years ago trying to simulate the formulas but gave up based upon my very limited math background. (This was well before Excel, MSDOS and Dual Floppy Drives).

So someone could probably whip up some spreadsheets with all the needed formulas.

Gerald
Parent - By Harman (*) Date 02-13-2015 19:55
Thanks Gerald.
Parent - - By Tyrone (***) Date 02-11-2015 11:51
Hey Harman,
Take a look at Edison Welding Institute's software:

http://ewi.org/ewi-weldpredictor-innovation-in-modeling-simulation/

Tyrone
Parent - By Harman (*) Date 02-13-2015 19:55
Thanks Tyrone. I have contacted them.