The CCT diagram I have shows an Ms at about 480°C, the curve moves upward as the time increase (more than about 10s). The 90% line lies at about 310° at times below 10 seconds but are over 400°C at 100 seconds. The Mf line is at about 180° at 10 seconds.
Hope this help