![](/mwf/attachments//avatars/100074480-9510.jpg)
Hello fellow welders,
I'm designing some parts that will have a variety of types of welds. Section 3.4 of D1.2 states "Each WPS shall be qualified by positioning and welding the test assembly in the manner stated below" and then lists the different types and positions. So does that mean that each WPS is contingent on ONE type and position of weld, or do all just need to conform to the code? Basically, if I have a CJP 1F weld and a PJP 1G weld on the same fabricated part, can they go on the same WPS, or do I need 2 separate tests?
Thanks,
Tori