The stainless steel pipe is to be used for guardrails around a dry dock. The main welding will be attaching a midrail to a U shaped piece, the U shapes piece being the posts and the top rail of the guardrail. Stainless steel pipe will also be welded to a stainless steel plate to anchor the guardrail. My impression is both cover by AWS D1.6 Thanks for your help.