- - By jwright650 (*****) Date 05-06-2015 14:55
Can anyone point me to a lab in the NY area that can determine the composition of some 3/8 diameter wire? Trying to help out an old high school classmate.
Parent - - By theweldor (*) Date 05-07-2015 01:42
I could get you a name of a place in Erie,Pa that does that kind of work. I am in Western NY so that isn't that far for me.
Parent - By jwright650 (*****) Date 05-11-2015 23:11
Thanks guys....she found a lab and should have her results soon.
Parent - By kcd616 (***) Date 05-07-2015 16:57
John,
have not done any here
wish I could help:sad:
internet search is best I can say
always here for you buddy
even if I am no help:wink:
sincerely,
Kent