![eek :eek:](/f2/epx.png)
You are kidding aren't you?!!
Welding is considered to be in the '
FLAT' position as long as it is within 15° of a 0° position. Just because it is called the angle of 'INCLINATION' does not mean it only applies to welding between 0 and 15° UPHILL. 0 - 15° DOWNHILL is still a FLAT position weld, with ANY process. And if you are talking about less than a 5° incline/decline it isn't even worth a consideration.
If I have understood the positioning and angles correctly... I have to side with the shop. It's flat.
Gotta be a CA DOT inspector.
He Is In Control, Have a Great Day, Brent