A 2 minute search found this on a steel supplier's website:
Heat Treatment
Annealing – Heat slowly to 1500 – 1650°F (816 – 899°C), cool to 1100oF (593°C) in furnace, air cool
Process Annealing – Heat to 1350 – 1450°F (732 – 788°C), air cool
Hardening – Heat to 1700 – 1850°F (927 – 1010°C), air cool or oil quench. Follow by stress-relief or temper
Stress Relieving – Heat to 300 – 800°F (149 – 427°C) for 1 to 2 hours, air cool
Tempering – Heat to 1100 – 1400°F (593 – 760°C) for 1 to 4 hours, air cool