Hi every body

I want to preparing sample on qualification of E7016, According to  table 4 of AWS A5.1.

1- For 3.2mm diameter all tests mentioned as NR. what's mean? testing is not required. how can get approval of my client?
2-When  V & OH mentioned for fillet test it means that fillet test sample shall be prepared in both positions?

THX
Parent - - By js55 (*****) Date 03-01-2016 15:34
Not sure what you mean by 'qualification' of E7018. The testing regimes in the AWS/SFA standards are for 'classification' of weld materials.
Parent - - By Jmaziyar (*) Date 03-02-2016 04:54
OK, qualification substitute by classification.  what's your idea on the subjects?
Parent - - By js55 (*****) Date 03-02-2016 13:51
What is it you are trying to do?
Parent - - By Jmaziyar (*) Date 03-05-2016 09:10
we use electrode out of our client vendor list.
for getting approval of our client, we are going to take qualification test
Parent - By js55 (*****) Date 03-07-2016 13:42
Keep in mind that the requirements of the A/SFA specifications ARE NOT filler metal 'qualification' requirements. They are simply requirements in order to label the filler metals with the specification identification.