The test is used to test large floor area welded seems. The boxes that I have seen has a metal frame with a rubber seal on the bottom and a clear plex-a-glass top. Hook air to the valve system causing a vacuum after you have sprayed the test area with a leak detector liquid. Hope this helps. I do not know what you want to know about this test.
Gary