- - By HokieGirl87 Date 03-08-2016 13:45
I have a 1-in. thick plate that I'm doing a WPS for and the sample is too big for our fixtures and/or load capabilities.  I don't see anything that says you can use a reduced size sample for 1-inch thick plate.  I only see that requirement for Table 4.9 steels.  This is ASTM A36 material so that wouldn't apply in this case.  Does anyone know if you can use a round sample for 1-inch thick plate?
Parent - By peterj357 (*) Date 03-08-2016 15:07
Figure 4.14 (in D1.1 2010) has the info for reduced-section tension specimens.