Couple questions
1) You say you have dispatched the job. Does this mean that your AI signed the Data Report and witnessed the stamping BEFORE raising these issues?
2) Did you have a requirement to control travel speed on your non CVN WPS?
The trick here is to write an NCR and qualify a procedure for CVN's using the parameters you already used in production.