Hey Art,
Sounds sorta like you are an independent contractor.
As mentioned... AWS D1.8 is a seismic supplement to the D1.1 Structural code for steel.
D1.8 does have some additional "situational" requirements for welder performance qualification testing (Welder Certs.)
"5.1.1 Required Tests. In addition to the requirements
of AWS D1.1/D1.1M Clause 4, welders shall pass the
Supplemental Welder Qualification for Restricted Access
Welding as prescribed in Annex D, when the welder is
required to make welds meeting all of the following
requirements:
(1) The weld is Demand Critical.
(2) The weld joins the bottom beam flange to the column
flange.
(3) The weld must be made by welding through a
beam web weld access hole.
If you are a contractor doing work to the specification, you should have your own copy of the latest D1.8 as there are also some fabrication details in splice transitions, and greater detail required in WPS's.
Here is one example of a restricted access performance qualification test assembly.