Sir,
Point By Point
I personally would enjoy talking about the bridge and all its anomalies with you
![cool :cool:](/f2/epx.png)
If you would be so kind as to single out one or two definite defects in the bridge structure, I'm sure you will find a lot of opinions on this site--including my own.
The material of construction "steel" of 1870 - 1880 !
A6 ??
Weld used with war conditions etc. 30's to 60's not "good practice"
Unknown metal fatigue quality control practices. The design engineer John Roebling put 15 % more cable as a control of corruption factor. It proofed accurate.
I'm sure that the members of the Society of Civil Engineers have virtual volumes of technical data on this particular bridge.
Member of ASCE - not that I am aware of.
It might be fun if you could attach more of what they have found with the fatigue cracking (there I go assuming it was fatigue)
Hard to come up with such. Rebuilds , modifications form about 1900 on. Trolley line on and off , rail on and off and and !
Could you also send us some pictures of the tacks? I'm having a hard time getting my mind around why someone would have left tacks on a bridge structure.
No ! It was a practice to tack weld the rivet to get a "temporary" strengthening.
It might have been those annoying heroin addicts you spoke of, I know that drugs are a big problem in the work force these days
![confused :confused:](/f2/epx.png)
I'll be looking forward to a repost from you on some particulars.
New York City with Supreme court decisions is challenging !
There were war time pressures and ignorance of welding. We learn a lot from more than 5000 welded ships built in the USA in four years about welding. Said ship were lost in considerable numbers without being analyzed. The bridge did not.
I'm assuming that the bridge is mostly riveted.
As built rivets and pins. When completed the largest man made object outside of Pyramids and Great Wall of China.
Can we hear more about the extent of the rework performed in the twenties.
Unaware of twenties work. War Department did major work 1943 - 1944 . A third of shipped to war went though New York harbor.
Ready for comments !
What exactly did they do?