I am trying to better understand the foot note d requirement in table 4.2 of AWS D1.1:2010 which states: "CJP groove weld qualification on any thickness or diameter shall qualify any size of fillet or PJP groove weld for any thickness or diameter."
So if I qualify a plate to plate CJP butt weld, then does that mean a fillet weld of any size around any diameter is also qualified? Seems to be inconsistent with the pipe diameter limitation for the fillet pipe T-test in table 4.4 (foot note c).
In a similar way does table 4.11 (foot note d) qualify a welder to weld any size fillet around any diameter if they have qualified a plate to plate CJP groove weld?
Thanks,
Brendan