Dear experts,
Can anyone clarify about AWS D1.6 table 4.2(b) ?. Table 4.2(b) states for the number of welds per that 1 weld test specimen for each position to be uesd.
In my interpret
If the PQR was tested in the "2F" position then the WPS is qualified for "2F" position only. Right ?