Yes, sir I can
for P-number qualification for welders - QW-423.1
for F-number qualification for welders - QW-433
For future reference what you can do is go to the following QW's for any information on the essential variables for a given process, afterwards you just have to follow the path to the other QW's it references
Welders:
QW-352 - OFW
QW-353 - SMAW
QW-354 - SAW
QW-355 - GMAW
QW-356 - GTAW
QW-357 - PAW
Procedures:
QW-252 - OFW
QW-253 - SMAW
QW-254 - SAW
QW-255 - GMAW
QW-256 - GTAW
QW-257 - PAW