Not logged inAmerican Welding Society Forum
Forum AWS Website Help Search Login
Up Topic Welding Industry / General Welding Discussion / welding
- - By Pejman Date 12-08-2016 22:56 Edited 12-10-2016 16:13
welding
Parent - - By 803056 (*****) Date 12-08-2016 23:06
Self imposed exile. I can respect that.
Parent - By kcd616 (***) Date 12-09-2016 05:33
how true
sincerely,
Kent
Parent - - By kcd616 (***) Date 12-09-2016 05:29
if people would
think before they make laws:eek::cool::yell:
the world would be better:yell::grin:
everyday just do no harm:cool::grin::yell:
and do your best:yell::yell::yell::yell:
and the world is a better place:yell::yell::yell::yell::yell::yell::yell::grin::cool:
sincerely,
Kent
Parent - By Cumminsguy71 (*****) Date 12-10-2016 21:18
Reese's.......
Parent - By tuanhai Date 02-17-2017 04:15
Thank for share
- - By gm007 Date 01-24-2017 04:40
hi,
I want to know that as per aws d1.1, pre-qualification of wps. do we need to approve pqr or approved wps?
Parent - - By jwright650 (*****) Date 01-24-2017 20:39
To be a pre-qualified wps, it must meet all of the criteria listed in AWS D1.1 Clause 3

If anything changes, and the change does not meet the criteria listed in Clause 3, then you will need to write a pqr and qualify the wps.
Parent - By Tommyjoking (****) Date 02-01-2017 02:15
you must prove you have no "stupid" allergy....if so you are prequalified for this job.
Up Topic Welding Industry / General Welding Discussion / welding

Powered by mwForum 2.29.2 © 1999-2013 Markus Wichitill