By DaLi64
Date 12-21-2016 08:58
The main purpose of the PWHT will be to remove as much hydrogen (subsea pipeline) as possible from the weld and the heat affected zone, but also for stress relief. In order to reduce the level of hydrogen in and adjacent to the weld, a large temperature should be used. However, a large temperature will adress critical issues like sensitization and a degraded clad-base interface. So it is not easy to chose such a temperature. A very complicated part of the weld is the so-called triple point where the weld material, base material and clad has a common interface. I must also add that I work on numerical simulations of welding, and to get input from knowledgeable people who have good experience from welding is valuable to me.