Dear Sirs
Base Material - API 5L X52
Test Position - 6GR- Fig 9.26
Weld Process- GTAW + FCAW & GTAW +GMAW ( 2 test Coupons )
When PQR Qualification performed in conformance with Fig 9.26 and Table 9.8 & 9.9, Does Mock Test required as mentioned in 9.15.4.1?
My understanding - Not Required
If required, please explain