i bet they burned holes w/ that. Recently I used 3/32 7014, it does a nice job, but you need to be very, very, very, in tune. there is no margin for not having the perfect, start, angle, arc length,motion etc. I found it difficult, the slag is also tricky
ive used nr211 .030 a couple times before, but had reasons not to on this job. thanks everyone for the time being, i may come back later for more advice