I did some test for welding 304L with pulse Mig. The plate thickness is 2.5mm, the wire is ER308LSi, 0.9mm Dia.
Welding position: Vertical up
Backup: Fibre Glass
Joint: Butt
I could not make a good weld.
Do you have ideas, suggestions? Any feed back will be appreciated.
Gong