Hello everyone!
I have a doubt about the root inspection of tension welds.
According to note 3 of table 6.3, welds classified as tension welds, shall have an increase of sensibility during scanning of the root face area.
My doubt is how to measure this area... I mean, how much of the joint is considered root. Here we have a double V joint, backgouged. My first thought is to consider the nose preparation.
Does anybody knows if there's a common sense about the subject?
Thanks a lot.