- - By DaLi64 Date 11-29-2017 09:37
Do anyone know where I can find (free) CCT and/or TTT diagrams for any of the following types of steels: X80, X65, X60, P235, P265, S460 and S420. I have been searching the internet without success. Grateful for any help.
Parent - - By 803056 (*****) Date 11-29-2017 11:44
They are protected by copyright, so I doubt you will find them.

Al
Parent - By DaLi64 Date 12-01-2017 10:32
Thanks, Al.
Parent - - By Tyrone (***) Date 11-30-2017 13:35
Takes tens of thousands of dollars to create.  It's the secret recipe for steel mills. They keep them near and dear.
Parent - By DaLi64 Date 12-01-2017 10:32
Thanks, Tyrone.