I was wondering if anyone could answer a question for me about a WPS. I was curious, if using one of the prequalified joints in D1.3, can a base metal from another code be used?
Thanks for the replies. I think I got it worked out. The base metal being used is out of ASME, but we are having to use D1.3 for the qualification(sheet). So, what I have found is that we will have to do a wps and a pqr for it. Thanks again and if anyone has anymore information they'd like to share, it is greatly appreciated.
Thanks for the replies and info.. So, let’s say for instance, I tested someone, welding a piece of 7 gauge to 12 gauge, that would also be the qualification range? That is what it is looking like to me, anyway. Thanks again for the help.
Thanks for the reply. I have looked at it. From what I read, if I qualify them on the thicker(7 ga.), they will be qualified from 16 ga. to 7 ga.? Thanks again for the info..