What's the effect of N2 on the Duplex material stainless steel ??? because my Client Specification for the shielding gas and purging gas shall be used Argon Nitrogen with mixture 98% Ar and 2% N2 (in my opinion the N2 for Good corrosion resistance and good for toughness. Is it true ???)
Thanks