Hi All,
For a job of mine, I have a WPS for the SMAW, overhead, uphill S355J2H to S355 J2H ( 3 mm to 32mm). But i have to change a secondary structure RHS 60x40,3mm from S355J2H to ASTM A500 due to the non-availability. This is being welded to S355J2H primary column structure and a plate of the same structure.
Can I use the same WPS S355J2H to S355 J2H or I need to qualify a different WPS for the different grades?