I'm not familiar with Armox? It sounds like it is hard and abrasion resistant. Do you have the chemistry of the base metal available? Did you contact the manufacturer to ask if they have any recommendations?
I did a quick Google search and see there are several alloys available. There are filler metal recommendations on their site that are specific to each alloy family.
Al