hi . when i was selecting the wire and shielding gas for armox plates i found that the ( stainless steel wire 307 si 1.2 and shielding gas is Ar 98 % and 2% O2)
i selected that according to handbook2016 KOBELCO and c1.10 lincoln elec So What i want know is that the best choose for consumable or is there better consumable for armox ??